IN718 nickel-chromium superalloy Powder
Product Details
| Morphology | Spherical, irregular | |||||
| Particles sizes | 0-20um,15-45um,15-53 μm,45-106um, 53-150um | |||||
| Powder Available for | • Additive Manufacturing (AM) • Metal Injection Moulding (MIM) Laser Cladding |
|||||
Chemical composition
| CHEMICAL COMPOSITION (WT%) | ||||||
| Ni | Fe | Cr | Nb | Mo | Ti | Co |
| 50-55 | Bal. | 17-21 | 4.75-5.5 | 2.8-3.3 | 0.65-1.15 | ≤ 0.1 |
| Al | Mn | Si | C | P | S | |
| 0.2-0.8 | ≤0.35 | ≤0.35 | ≤0.08 | ≤0.015 | ≤ 0.015 | |
Applications
• high-stress, high-temperature aeronautical, Aerospace
• Gas turbine blades,auto racing environments
• Exhaust manifolds
• Rocket motors
• Heat exchangers